Title

Optical Properties Of Epitaxial Single-Crystal Chemical-Vapor-Deposited Diamond

Keywords

Calorimetry; CVD diamond; Depolarization loss

Abstract

Epitaxial single-crystal chemical-vapor-deposited diamond was obtained from Element Six Ltd. (Ascot, UK) and from Apollo Diamond (Boston, MA). Both companies provided 5 × 5 mm squares with thicknesses ranging from 0.5 to 1.5 mm. In addition, Element Six provided 10-mm-diameter disks with a thickness of 1.0 mm. The absorptance of all specimens at 1064 nm was measured by laser calorimetry, with good agreement between independent measurements at the University of Central Florida and at QinetiQ (Malvern, UK). Depolarization at 1064 nm and ultraviolet absorption properties are also reported.

Publication Date

11-6-2007

Publication Title

Proceedings of SPIE - The International Society for Optical Engineering

Volume

6545

Number of Pages

-

Document Type

Article; Proceedings Paper

Personal Identifier

scopus

DOI Link

https://doi.org/10.1117/12.718365

Socpus ID

35648960815 (Scopus)

Source API URL

https://api.elsevier.com/content/abstract/scopus_id/35648960815

This document is currently not available here.

Share

COinS